Rhenium

Element density: 21.02 g/cm3
Electron configuration: [Xe]4f145d56s2
Oxidation states: +4,67

Rhenium

Edges

Explore electron energy loss spectroscopy (EELS) reference spectra, featuring major and minor edges used for elemental identification and chemical state analysis in materials research. 
 

 

Major edges

L3

10535

 

 

M4

1949

 

Major_Delayed Minimum

M5

1883

 

Major_Delayed Minimum

O2

46

Minor_Broad Peak
Major_Delayed Minimum

O3

35

Minor_Broad Peak
Major_Delayed Minimum

 

Minor edges

L1

12527

 

 

L2

11959

 

 

M1

2932

 

Very Weak_Abrupt Onset

M2

2682

Very Weak_Sharp Peak
Very Weak_Delayed Minimum

M3

2367

Minor_Sharp Peak
Minor_Delayed Minimum

N1

625

 

Very Weak_Abrupt Onset

N2

518

Intermittent_Sharp Peak
Very Weak_Delayed Minimum

N3

444

Intermittent_Sharp Peak
Very Weak_Delayed Minimum

N4

274

 

Minor_Very Delayed

N5

260

 

Minor_Very Delayed

N6,7

41

 

 

O1

83

 

Very Weak_Abrupt Onset

Enhance your EELS community

Share spectra with your fellow EELS users from around the world.

Related spectral data

Re(0-0180eV)
   

Re electropolished foil (0 – 180 eV)

Material analyzed: Re

Related elements: Rhenium

Data contributor: Gatan

Beam energy (keV): 200

Nominal energy range (eV): 0 – 180

Collection semi-angle effective (mrad): 100

 

Notes: Serial EELS; 10 sweeps 20 ms dwell 

 

Re electropolished foil (0 – 3870 eV)
   

Re electropolished foil (0 – 3870 eV)

Material analyzed: Re

Related elements: Rhenium

Data contributor: Gatan

Beam energy (keV): 200

Nominal energy range (eV): 0 – 180

Collection semi-angle effective (mrad): 100

 

Notes: Serial EELS; zero-loss peak intensity = 5.15e9; total elastic int. / zero-loss int. = 0.53; gain change factor = 229; 150 sweeps 10 ms dwell 

 