EELS | AMETEKSkip to Main Content
No options found

Cesium

Element density: 1.88 g/cm3
Electron configuration: [Xe]6s1
Oxidation states: +1

Cesium

Edges

Explore electron energy loss spectroscopy (EELS) reference spectra, featuring major and minor edges used for elemental identification and chemical state analysis in materials research. 

 

 

Major edges

L3

5012

 

 

M4

740

Major_Sharp Peak
Major_Delayed Minimum

M5

726

Major_Sharp Peak
Major_Delayed Minimum

N4

79

Major_Broad Peak
Major_Delayed Minimum

N5

77

Major_Broad Peak
Major_Delayed Minimum

O2

13

 

 

O3

11

 

 

 

Minor edges

L1

5715

 

 

L2

5359

 

 

M1

1217

 

Very Weak_Abrupt Onset

M2

1065

Intermittent_Sharp Peak
Very Weak_Delayed Minimum

M3

998

Intermittent_Sharp Peak
Very Weak_Delayed Minimum

N1

231

 

Very Weak_Abrupt Onset

N2

172

Intermittent_Sharp Peak
Very Weak_Delayed Minimum

N3

162

Intermittent_Sharp Peak
Very Weak_Delayed Minimum

O1

23

 

 

 

Considerations

If you have data that you would like to share with this EELS community, please feel free to use the link below to submit your data for consideration.

Enhance your EELS community

Share spectra with your fellow EELS users from around the world.

Related spectral data

CsF particles on a thin C film (0 – 180 eV)
   

CsF particles on a thin C film (0 – 180 eV)

Material analyzed: CsF

Related elements: Cesium, Fluorine

Data contributor: Gatan

Beam energy (keV): 120

Nominal energy range (eV): 0 – 180

Collection semi-angle effective (mrad): 13

 

Notes: Serial EELS; mass loss during acquisition; zero-loss peak intensity = 2.54e8; total elastic int. / zero-loss int. = 0.20; gain change factor = 3192

 

CsF particles on a thin C film (0 –890 eV)
   

CsF particles on a thin C film (0 – 890 eV)

Material analyzed: CsF

Related elements: Cesium, Fluorine

Data contributor: Gatan

Beam energy (keV): 1

Nominal energy range (eV): 0 – 890

Collection semi-angle effective (mrad): 0

 

Notes: Serial EELS; scaled by 0.9 for plotting

 

CsI particles on thin C film (0 – 180 eV)
   

CsI particles on thin C film (0 – 180 eV)

Material analyzed: Csl

Related elements: Cesium, Iodine

Data contributor: Gatan

Beam energy (keV): 120

Nominal energy range (eV): 0 – 180

Collection semi-angle effective (mrad): 2

 

Notes: Serial EELS; zero-loss peak intensity = 2.2e9; total elastic int. / zero-loss int. = 0.15; gain change factor = 8174; mass loss during acquisition; zero-loss ok

 

CsI particles on thin C film (0 – 990 eV)
   

CsI particles on thin C film (0 – 990 eV)

Material analyzed: Csl

Related elements: Cesium, Iodine

Data contributor: Gatan

Beam energy (keV): 120

Nominal energy range (eV): 0 – 990

Collection semi-angle effective (mrad): 2

 

Notes: Serial EELS; low-loss saturated

 

Looking for more Information

Want to enhance your EELS results?

Visit EM Academy to stream lessons from application specialists and design engineers anytime, anywhere, and at your own pace.